MIL-DTL-14824C(AR)
3.9.5 Foreign matter. No part of the assembly shall contain
dirt, grease, chips, rust, corrosion or other foreign matter.
3.9.6 Protection of rotating band. The machined rotating
band shall be protected from being nicked, burred or otherwise
damaged in subsequent handling prior to shipment.
3.10 Ballistics test. The projectile assembly shall reveal
no evidence of metal parts failure. Metal parts failure shall be
defined as:
3.10.1 Deformation. There shall be no projectile body
deformation as evidenced by rifling marks extending more than 180
degrees around the body.
3.10.2 Breakup. There shall be no loss or breakup of metal
parts components in the gun bore or in flight.
3.10.3 Rotating band failure.
There shall be no loss or
fanning of the rotating band.
3.10.4 Shearing of rotating band. There shall be no shear
of rotating band as evidenced by complete lack of engraving.