MIL-DTL-60377C (AR)
3.5.7.2 Sum. Not more than one transverse crack shall be
permitted in Segment A and not more than two transverse cracks
shall be permitted n Segment A, B and C combined. Cracks which
appear to be joined at any point shall be considered as one
crack. Transverse cracks on x-ray film or display appear as a
group or cluster of lines or elements because the crack in the
explosive is fragmented along various fracture lines. An
apparent collection of such transverse elements that are
joined together shall be considered as one crack. Separated
transverse cracks apparently joined by a longitudinal crack,
know as "Christmas tree" cracks, shall be counted as separate
cracks.
3.5.8 Annular ring. An annular ring within the explosive
charge shall not exceed the requirements specified in Table I.
6